Ball milling media
Zirconia ceramic beads with proportion of 6.0 can be used as specifications 0.2mm-30mm
Main chemical composition:ZrO2 94.6% Y2O3 5.4%
True specific gravity:: 5.9-6.1g/cm3
Apparent specific gravity: 3.7g/cm3
Moh's hardness : ≥9
Flexure strength: ≥1000Mpa
Breaking tenacity : 12~14Mpa.m1/2
Color: Pearl color white
Package: plastic bucket or woven bag
English name: TZP Zirconia Ceramic Beads